Title: | Electrically Conductive Biocomposites Based on Poly(3-hydroxybutyrate-co-3-hydroxyvalerate) and Wood-Derived Carbon Fillers | Authors: | Unterweger, Christoph Ranzinger, Matija Duchoslav, Jiri Piana, Francesco Pašti, Igor Zeppetzauer, Franz Breitenbach, Stefan Stifter, David Fürst, Christian |
Keywords: | biocarbon;biocomposites;electrical conductivity;mechanical properties;PHBV | Issue Date: | 1-Aug-2022 | Journal: | Journal of Composites Science | Abstract: | In this paper, biobased carbons were used as fillers in poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV). The mechanical and electrical properties of these 100% biocomposites were analyzed. First, biocarbons were prepared from wood dust and cellulose fibers using carbonization temperatures ranging 900–2300 °C. XRD revealed significant improvements of the graphitic structure with increasing temperatures for both precursors, with slightly higher ordering in wood-dust-based carbons. An increase of the carbon content with continuous removal of other elements was observed with increasing temperature. The carbonized cellulose fiber showed an accumulation of Na and O on the fiber surface at a carbonization temperature of 1500 °C. Significant degradation of PHBV was observed when mixed with this specific filler, which can, most probably, be attributed to this exceptional surface chemistry. With any other fillers, the preparation of injection-molded PHBV composites was possible without any difficulties. Small improvements in the mechanical performance were observed, with carbonized fibers being slightly superior to the wood dust analogues. Improvements at higher filler content were observed. These effects were even more pronounced in the electrical conductivity. In the range of 15–20 vol.% carbonized fibers, the percolation threshold could be reached, resulting in an electrical conductivity of 0.7 S/cm. For comparison, polypropylene composites were prepared using cellulose fibers carbonized at 2000 °C. Due to longer fibers retained in the composites, percolation could be reached in the range of 5–10 vol.%. The electrical conductivity was even higher compared to that of composites using commercial carbon fibers, showing a great potential for carbonized cellulose fibers in electrical applications. |
URI: | https://dspace.ffh.bg.ac.rs/handle/123456789/67 | DOI: | 10.3390/jcs6080228 |
Appears in Collections: | Journal Article |
Show full item record
SCOPUSTM
Citations
4
checked on Dec 29, 2024
Page view(s)
28
checked on Jan 4, 2025
Google ScholarTM
Check
Altmetric
Altmetric
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.